Вернуться к статье

LABORATORY TESTS FOR INCREASING THE ICE-FORMING EFFICIENCY OF AD1 CRYSTALLIZING AGENT WITH THE ADDITION OF ZINC OXIDE NANOTUBES

Figure 1 - (T-x)-section of the phase diagram of the binary system Zn–O at a pressure of 0.1 MPa

(T-x)-section of the phase diagram of the binary system Zn–O at a pressure of 0.1 MPa

L denotes the solubility of oxygen in Zn at different temperatures. Tm(Zn) – melting point of zinc (419.6 ºС)