Лабораторные исследования влияния реагента на основе кластеров оксида цинка на туманы
Table 2 - Concentrations of 0.3-1 micron droplets before and after exposure to ZnO
Background concentration values | 3 minutes after applying the reagent | ||||||||||||
µ tº | 0,3 | 0,5 | 1 | 5 | 10 | 25 | µ
tº | 0,3 | 0,5 | 1 | 5 | 10 | 25 |
+1 | 22,5×106 | 30,9×106 | 21,3×106 | 960 | 240 | 0 | +1 | 14,1×106 | 30,4×106 | 39,6×106 | 16199 | 600 | 0 |
+2 | 10,8×106 | 25,0×106 | 69,3×106 | 5161 | 840 | 0 | +2 | 17,1×106 | 31,8×106 | 32,2×106 | 5278 | 360 | 0 |
+3 | 28,1×106 | 31,0×106 | 16,7×106 | 2521 | 0 | 0 | +3 | 26,5×106 | 38,3×106 | 12,0×106 | 9242 | 840 | 0 |
+4 | 13,5×106 | 31,0×106 | 41,1×106 | 1580 | 100 | 40 | +4 | 27,4×106 | 34,7×106 | 14,3×106 | 43400 | 4840 | 160 |
+5 | 25,2×106 | 29,0×106 | 20,6×106 | 960 | 80 | 0 | +5 | 24,1×106 | 35,4×106 | 16,8×106 | 21580 | 1700 | 60 |
+6 | 13,0×106 | 30,7×106 | 47,1×106 | 1939 | 240 | 0 | +6 | 10,4×106 | 24,9×106 | 69,3×106 | 24058 | 1340 | 20 |
+7 | 39,0×106 | 32,8×106 | 6,7×106 | 440 | 140 | 0 | +7 | 22,7×106 | 38,5×106 | 17,4×106 | 36904 | 3140 | 120 |
+8 | 11,1×106 | 26,1×106 | 66,7×106 | 2600 | 300 | 20 | +8 | 10,2×106 | 24,6×106 | 71,0×106 | 24462 | 1440 | 20 |
+9 | 31,4×106 | 32,5×106 | 13,8×106 | 4680 | 360 | 0 | +9 | 9,5×106 | 23,0×106 | 75,4×106 | 28418 | 2680 | 0 |
+10 | 5,8×106 | 7,5×106 | 90,7×106 | 0,2×106 | 140 | 20 | +10 | 4,1×106 | 94419 | 77,9×106 | 6,4×106 | 1180 | 0 |