Thermodynamic and Structural Cu-Sn-Zn Alloy Properties
Table 1 - Difference of the Components' Chemical Potentials and the Gibbs energies in the hardened and annealed Cu-Sn-Zn alloy specimens at Т = 295 К (J/mole)
|
|
|
|
480 ± 100 | 2390 ± 150 | 1850 ± 140 | 710 ± 90 |